Pint $32.55
Designed with the potter in mind, capable of producing an infinite variety of colors and surfaces (by layering) and even reduction effects in oxidation! To use these glazes is to step into different ceramic glaze traditions of many cultures throughout history. Optimal results at Cone 5/6. A powerful advantage of this product line is the outstanding support provided by the manufacturer. The web page at the AMACO website (click above) has very good documentation (especially charts) about all the layering possibilities, it will save you alot of testing. These glazes are not guaranteed to be fit Plainsman bodies. For functional surfaces thermal-shock ware (boiling water soak to ice water soak, and then back) to make sure they do not craze or shiver. P300 is most likely to craze, M340 and M390 are least likely. We do ongoing testing and are adding pictures of these used on our products.
AMACO PC-32 (right) compared to an Alberta Slip brown made using only frit, iron and tin oxide. The former employs lithium carbonate (the reason for its higher cost). The body is M332.