742 Dark Red

Pint $20.00 ea

Gallon size available on special order.

Type: Spectrum Opaque Gloss Low Fire Glazes

Canadian made. Leadless. Cone 06 - 04. Excellent lead free, dinnerware safe, A/P non-toxic clear glaze. Compatible with most commercially available underglazes. Good tolerance for a wide variety of low fire pugged bodies and rarely crazes (for castware, consider trying 400 Clear or 800 Clear). Brush 1 to 2 coats (may cloud when applied too heavily). 701-763 - Require 2 to 3 coats for opaque coverage. In general, a more even appearance can be achieved by alternating the direction of brush strokes. These glazes do not bleed together very much.

Manufacturer: Spectrum


Spectrum 742 Dark Red on L213 at cone 03