Plainsman GrogDescriptionHigh temperature buff burning brick micro-aggregate A fine inert aggregate made by grinding high temperature light buff burning construction brick. The product has dense, hard grains. The particles have approx 5% porosity by weight. Approximately 65% of the material spans a range of sizes from plus 48 mesh (300 microns) to 200 mesh (75 microns). The remaining 35% is less than 200 mesh. ![]() This material contains particle sizes that span the plus 200 mesh range (35% is also minus 200 mesh). This material is available in 20 kg bags and bulk bags (2000 lb). Physical PropertiesSieve Analysis (Tyler mesh): +48 (+300 microns): 1-5%
48-65 (200-300 microns): 15-20%
65-100 (150-200 microns): 25-30%
100-150 (100-150 microns): 5-15%
150-200 (75-100 microns): 5-15%
-200 (-75 microns): 30-40%Safety Data SheetClick here for web view. |
![]() |
Plainsman Clays 671 Industrial Ave. SE, Medicine Hat, Alberta T1A 3L5 Phone: 403-527-8535 FAX:403-527-7508 Email: tim.lerner@plainsmanclays.com |