G2934 Cone 6 Matte Base Glaze
G2926B Cone 6 Clear Glossy Base Glaze
GA6-B Alberta Slip Cone 6 Base
L3954B Mid Temperature Engobe
G1916Q Transparent Base Glaze
G1947U Transparent Base - Cone 10R
G2571A MgO Matte Base - Cone 10R
GR10-A Ravenscrag Slip as-a-glaze - Cone 10R
L3954N/J Cone 10 Engobe Base
| Glazes and Glaze Recipes - PlainsmanFood SafetyOur base glazes do not contain hazardous ingredients. They are resistant (as bases) to leaching tests in our circumstances. However when you fire them and you add stains, opacifiers, variegators then you are creating something different. Please do your own leaching test.
Before using any of these on a kiln load of ware: Read the documentation. Test first on the clay you intend to use it on. When mixing, screen them to assure a defect-free surface. About Our Base Glazes
Variegating Colored SurfacesIt is usually possible to variegate a colored glaze by adding some rutile or titanium (2-5%). Since the former contains iron, it can muddy lighter colors. |
![]() |