Main Categories → Amaco Potter's Choice Medium Fire → Clays → High Temperature Clays
High Temperature Clays
Plainsman H440 Info SDS
Red-brown burning cone 10R speckled iron body.
box: $34.95
Plainsman H441G Info SDS
Light burning cone 10R speckled iron sculpture body.
box: $31.10
Plainsman H443 Info SDS
Brown burning cone 10R speckled iron body.
box: $37.25
Plainsman H550 Info SDS
Speckled slightly sandy cone 10R buff stoneware.
box: $31.90
Plainsman H555 Info SDS
Very lightly speckled smooth cone 10R porcelainous stoneware.
box: $46.95
Plainsman H570 Info SDS
Clean burning cone 10R whiteware.
box: $54.75
2.5kg bag: $8.30
Plainsman Sculpture Clay Info SDS
Dark burning vitreous plastic highly grogged cone 10R speckled iron sculpture body.
box: $47.60