M340 Casting
Print

M340 Casting

Description

Code numbered L3798G. A casting body that is of similar color and maturity to M340 (but made from refined materials). We do not produce this as a product, but publish its recipe and preparation information. It is important to understand the principles of deflocculation, be able to measure specific gravity effectively and have a good propeller mixer.

Firing


M340 Casting fired bars (cone 4 to 8 bottom to top). The porosity is 2.5% at cone 6, the same as regular M340. Firing to cone 7 reduces it to 1.5%.

Gallery


M340 Casting - Mugs were cast and then finished on the jigger wheel. The inside glaze is G2026B, outside is G2934Y black and G2926B white (with speck added).

Safety Data Sheet

Click here for web view.

Logo Plainsman Clays
671 Industrial Ave. SE, Medicine Hat, Alberta T1A 3L5
Phone: 403-527-8535 FAX:403-527-7508
Email: tim.lerner@plainsmanclays.com