G2934 Cone 6 Matte Base Glaze
G2926B Cone 6 Clear Glossy Base Glaze
GA6-A/B Alberta Slip Cone 6 Base
GR6-A Ravenscrag Cone 6 Base
L3954B Mid Temperature Engobe
G1916Q Transparent Base Glaze
G1947U Transparent Base - Cone 10R
G2571A MgO Matte Base - Cone 10R
GR10-A Ravenscrag Slip as-a-glaze - Cone 10R
L3954N/J Cone 10 Engobe Base
| G2571A MgO Matte Base - Cone 10RDescriptionA balanced dolomite matte for reduction firing (although it works well in oxidation also). It is better than any other dolomite recipe we have ever used.
For lots of detail visit the page for this G2571A at the Digitalfire Reference Database. GlazingWhen mixed with water to create a thixotropic slurry, this will perform was as a dipping glaze. It will apply evenly to bisque, produce minimal dripping and dry within seconds. It will be adequately durable for handling. If bisque walls are thin, it will be necessary to glaze the inside and outside of pieces as separate operations (with a drying time between). If you are glaze laying (using this as a dipping glaze and painting a commercial gummed brushing glaze over it) there is a risk of crawling. It may be necessary to add some gum to this, converting it from a dipping glaze to a base-coat dipping glaze. RecipeAs of Apr 2018 it is not yet available as a premixed product. However you can make it yourself, click the following: G2571A (for the recipe and much more). Gallery![]() Left: G2571A magnesia matte glaze on H440 fired at cone 10R. Right: GR10-J is the same glaze (having the same chemistry) but made using Ravenscrag Slip to supply much of it. ![]() G2571A cone 10R matte on H450 mugs. Bamboo version on left has 3.5 Rutile and 10 Zircopax added. Both mugs had L3954N black engobe applied inside and half way down the outside during leather hard stage. The liner glaze on the left is pure Ravenscrag Slip GR10-A. ![]() Laguna B-Mix with G2571A bamboo over L3954J black engobe. The black engobe bleeds through as brown on the bamboo but black on the liner glaze (GR10-C Ravenscrag talc matte). ![]() H441G thrown cylinders with G2571A liner glaze. The right-most cylinder has L3954H white engobe under the glaze. Safety Data SheetClick here for web view. |
![]() |
Plainsman Clays Ltd. 702 Wood Street, Medicine Hat, Alberta T1A 1E9 Phone: 403-527-8535 FAX:403-527-7508 Email: plainsman@telus.net |