Main Categories
Plainsman * Snow * Info SDS
Our Brightest and Whitest burning earthenware. Made from refined dolomite, ball clay and bentonite. This clay is also available in a dry version which is intended for slip casting. This clay body replaces former Talc based clays such as L213.
box: $46.45
Plainsman 98 Mix Dry Clay Info SDS
Low fire high iron plastic clay. Also recommended as a mortar and cover materials for thermal mass ovens.
50# Bag: $27.80
Plainsman Buffstone Info SDS
A slightly sandy, buff burning, medium plasticity body.
box: $28.45
Plainsman Coffee Info SDS
Smooth, plastic, very dark burning cone 6 stoneware.
box: $49.05 ea
Plainsman Fireclay (Plainsman) Info SDS
A refractory and and plastic clay.
2.5kg bag: $4.90
22.68kg: $28.65
Plainsman FireRed Dry Clay Info SDS
High fire red fire clay
22.68kg bag: $43.95
Plainsman H440 Info SDS
Red-brown burning cone 10R speckled iron body.
box: $31.60
Plainsman H441G Info SDS
Light burning cone 10R speckled iron sculpture body.
box: $27.15
Plainsman H443 Info SDS
Brown burning cone 10R speckled iron body.
box: $34.20
Plainsman H450 Info SDS
Lightly speckled smooth cone 10R buff stoneware.
box: $38.30
Plainsman H550 Info SDS
Speckled slightly sandy cone 10R buff stoneware.
box: $28.45
Plainsman H555 Info SDS
Very lightly speckled smooth cone 10R porcelainous stoneware.
box: $39.95
Plainsman H570 Info SDS
Clean burning cone 10R whiteware.
box: $48.20
2.5kg bag: $7.90
Plainsman L210 Info SDS
Brown burning earthenware.
box: $27.50
Plainsman L212 Info SDS
Buff burning talc earthenware.
box: $41.85
Plainsman L215 Info SDS
Red burning very plastic earthenware clay.
box: $33.30
Plainsman M2 Clay Info SDS
High iron medium fire stoneware raw clay
20kg box: $40.55
Plainsman M332 Info SDS
Very sandy and plastic brown burning stoneware.
box: $29.60
Plainsman M332G Info SDS
Grogged brown burning sculpture clay.
box: $29.15
Plainsman M340 Info SDS
Smooth buff burning stoneware. Our most popular clay body.
box: $29.75
Plainsman M340GS Info SDS
Lightly grogged buff burning stoneware with manganese speckle.
box: $32.35
Plainsman M340S Info SDS
Smooth buff burning stoneware with manganese speckle.
box: $29.65
Plainsman M350 Info SDS
Smooth tan burning stoneware.
box: $33.25
Plainsman M370 Info SDS
Plastic white burning stoneware.
box: $47.25
2.5kg bag: $7.80
Plainsman M390 Info SDS
Smooth red burning stoneware, our most popular dark burning body.
box: $35.50
Plainsman Midstone Dry Clay Info SDS
Medium fire stoneware raw material
22.68kg bag: $29.45
Plainsman Modeling Clay
A plastic body not intended for firing. Varied consistency, scrap clay, low temperature only.
box: $28.45
Plainsman MSCULP Info SDS
Heavily grogged version of M340.
box: $38.75
PlastiSial (Buff) - Vallauris (Red) Self Hardening Clay
Available as "Vallauris", in a Red-brown color, or as "Plasti-Sial", in a light grey color. Air drying, and self hardening clay. Decorate with tempra or acrylic paints.
20kg box - Buff: $63.30
5kg bag - Buff: $15.80
20kg box - Red: $65.10
5kg bag - Red: $16.30
Plainsman Raku/Throwing Info SDS
Fired bars shown are cone 10R (top), 11, 10, 9, 8 oxidation (downward).
box: $40.25
Plainsman Ravenscrag Slip Info SDS
A natural clay that melts at cone 10R to form a silky white matte glaze. Add frit to melt at cone 6.
2.5kg bag: $8.15
20kg bag: $51.15
Plainsman Redstone Dry Clay Info SDS
Native high iron stoneware
22.68kg bag: $42.10
Plainsman Sculpture Clay Info SDS
Dark burning vitreous plastic highly grogged cone 10R speckled iron sculpture body.
box: $37.60